Tested the white pla pro one only a little doesnt feed great very picky for the mags. This one is pa6cf .6 nozzle 9 hour print. annealed for 14 hours will test soon.

    • Deadtroll@forum.guncadindex.comOP
      link
      fedilink
      English
      arrow-up
      2
      ·
      2 months ago

      these are new settings im working on with a .6 nozzle. my .4 nozzle settings are for the qidi Q2 at 320c and theyre on the sea under my same tag here. Theyre a remix of 300blkfdes settings he uses a bambulab

      • Knobgoblin@forum.guncadindex.com
        link
        fedilink
        English
        arrow-up
        1
        ·
        2 months ago

        I’ve used 300blkfdes settings and I’m not a huge fan maybe it the filament by nature but it always seems to come out really rough like sandpaper.

        • Deadtroll@forum.guncadindex.comOP
          link
          fedilink
          English
          arrow-up
          2
          ·
          2 months ago

          Make your outer line width thinner and that should help. I mean it’s pa6 it’s gonna be rough. sand it then hit it with a torch lighter that helps