In the construction of a FTN.5/4.5/4/3, etc is it recommended to anneal the PA6-CF? It seems it looses some of it’s impact resistance and flex but temperature resistance increases and also becomes stiffer and slightly more brittle. I’m assuming it’s recommended but just wanted to verify. Thanks!


cool… once i get my qidi plus 4 gears cleaned, i may try to print something in pps-cf.
i may also try plain pps…
If you do, let me know how it goes.
Recently someone had posted an interesting chart on this thread https://forum.guncadindex.com/post/forum.guncadindex.com/171322
And that seemed to be pretty telling. It sound like PPS-CF may be substantially inferior to PA6CF on some properties