help-circle


  • I use a cheap ninja 6qt that maxes out on dehydrator mode at 195f for 12-24h on new rolls, and print from a polymaker drybox with the 5% air exchanger mod stacks between the heater base/boxes. I also opened the heater + snipped out the plastic mesh, then super glued some SS mesh in its place, as recommended by the air exchanger designer. No issues with pa6, paht, ppa fibreheart, or pps. Less dry time for less hydroscopic materials like ppa, more time on the opposite end of the spectrum like pa6